MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin PX9406 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Water Absorption 0.060 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 75.0 MPa50 mm/min; ASTM D638
Elongation at Break 18 %50 mm/min; ASTM D638
Elongation at Yield 9.5 %50 mm/min; ASTM D638
Flexural Strength 111 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2640 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 160 JASTM D256
Izod Impact, Unnotched 1121 J/mASTM D4812
Dart Drop, Total Energy 42.0 Jpeak; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+16 ohmASTM D257
Dielectric Constant 2.49
@Frequency 1e+6 Hz
ASTM D150
 2.57
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 18.8 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.0026
@Frequency 1e+6 Hz
ASTM D150
 0.0052
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=0.750 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=0.750 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 133 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 150 °CRate B/50; ASTM D1525
UL RTI, Electrical 110 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 110 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.750 mm
UL 94
 5VA
@Thickness >=2.50 mm
UL 94
Glow Wire Ignition Temperature 775 °C
@Thickness 3.00 mm
IEC 60695-2-13
 775 °C
@Thickness 2.50 mm
IEC 60695-2-13
 775 °C
@Thickness 1.50 mm
IEC 60695-2-13
 775 °C
@Thickness 1.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 960 °C
@Thickness 2.50 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 305 °C
Zone 2 255 - 300 °C
Zone 3 265 - 305 °C
Melt Temperature 275 - 305 °CInjection Molding
Mold Temperature 70.0 - 100 °C
Drying Temperature 105 - 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Vent Depth 0.00380 - 0.00510 cm
Screw Speed 20 - 100 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82456 / 290403

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.