MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AGC FL1700 PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Product Description: FL1700 is a white PTFE (polytetrafluoroethylene) micropowder which is suitable as an economical, general-purpose dry lubricant in rubber and plastics compounding, and grease applications. FL1700 particles are coarse and friable. Some size reduction of the larger particles will occur during compound. FL1700 is suitable for use in food contact applications.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.530 g/ccASTM D4894
Particle Size <= 2.0 µmHegman; ASTM D1210
 <= 25 µmD10, Low Shear
 95 µmAverage, Low Shear
 <= 150 µmD90, Low Shear
Specific Surface Area 3.1 m²/gKrypton
 
Thermal PropertiesOriginal ValueComments
Melting Point 334 °CASTM D3417
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ASTM D4019

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Baystar™ 7195 High Density Polyethylene, Specialty Extrusion Resin
Zeus PVDF Tubing and Drawn Fiber
Zeus FEP Tubing and Drawn Fiber
Samyang Trirex® 3026PJ Polycarbonate
Plastcom PLASTALEN® PQ 82 N Polypropylene with improved impact strength

PAGCX123 / 191232

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.