MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Silres® SY 409 Silicone Resin
Categories: Polymer; Thermoset; Silicone

Material Notes: SILRES® SY 409 is a methylphenyl group containing silicone resin solution that is recommended as a binder for medium solids or high solids heat resistant paints in combination with other organic resins.

Application: SILRES® SY 409 is highly suitable for introducing a compatible silicone component into other binder systems to increase the weathering or heat resistance. Application examples are:

  • oven and stoves
  • industrial coatings
  • engine parts

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³
Solids Content 74 - 76 %
@Treatment Temp. 200 °C,
Time 3600 sec
74 - 76 %
@Treatment Temp. 392 °F,
Time 1.00 hour
Viscosity 50 - 150 cP50 - 150 cPdynamic; DIN 51562
 
Thermal PropertiesMetricEnglishComments
Flash Point 26.0 °C78.8 °FDIN 51755
Ignition Temperature 460 °C860 °FDIN 51794
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Appearanceclear solution
Content1.5-4.5%Hydroxyl group

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 49090R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Rogers Arlon 32400N060 0.060" (1.52 mm) Uncured Silicone Rubber
Rogers Arlon 32300R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier
Rogers Arlon 32090R028 Silicone Rubber Laminate
Parker Chomerics CHO-BOND® 1055, Part A Silicone Resin Mixture

PWACK9588 / 205117

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.