MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LG Chemical LG PVC LP010F poly vinyl chloride homopolymer
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: General LG Chem LP010F is a poly vinyl chloride homopolymer suitable for low viscosity plastisol processing.

Main Applications:

  • Top layer of flooring, Artificial leather
  • Technical textiles (tarpaulins, banners, conveyor belts)
  • Toy & Ball, Label
  • Cap closures & Can coating, Coil coating
Colorless coatings with LP010F shows crystal clear and glossy surface.

Advantages:

  • Very low initial viscosity
  • High transparency, glossy and crystal clear films
  • Lowest water absorption tendency
  • Excellent air release

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.300 - 0.380 g/cc0.0108 - 0.0137 lb/in³ASTM D 1895-90
Volatiles <= 1.2 %
@Temperature 110 °C,
Time 3600 sec
<= 1.2 %
@Temperature 230 °F,
Time 1.00 hour
ASTM D3030
Viscosity 3000 - 6000 cP3000 - 6000 cPB.F, DOP 60part,6rpm; ASTM D1824
Viscosity Measurement >= 1.0>= 1.0[g/sec], S.V, DOP 60part,4bar; ASTM D1823
 
Mechanical PropertiesMetricEnglishComments
K Factor (Wear Factor) 75 - 7775 - 77ISO 1628-2
 
Descriptive Properties
Degree of polymerization1600-170030?, JIS K 6720-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLHCHEM9928 / 239444

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.