MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Appeel® 20D875 Ethylene Acrylate
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temperature range to a number of container materials including PP, PS, PET and PVC. Appeel® 20D875 is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins.

Appeel® 20D875 Lidding Sealant Resin complies with Food and Drug Administration Regulation 21 CFR 175.105 - - Adhesives. This Regulation describes adhesives that may be used as components of articles intended for use in packaging, transporting, or holding food, subject to the limitations and requirements therein.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccASTM D792, ISO 1183
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 98.0 °CASTM D3418, ISO 3146
Vicat Softening Point 60.0 °CASTM D1525, ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 285 °C
Feed Temperature 140 °CBlown Film Coextrusion
 180 °CExtrusion Coating
Zone 2 150 °CBlown Film Coextrusion
 230 °CExtrusion Coating
Zone 3 160 °CBlown Film Coextrusion
 260 °CExtrusion Coating
Zone 4 180 °CBlown Film Coextrusion
 270 °CExtrusion Coating
Zone 5 180 °CBlown Film Coextrusion
 270 °CExtrusion Coating
Adapter Temperature 180 °CBlown Film Coextrusion
 270 °CExtrusion Coating
Die Temperature 170 °CBlown Film Coextrusion
 270 °CExtrusion Coating
Melt Temperature 150 - 190 °CBlown Film Coextrusion
 235 - 270 °CExtrusion Coating
Dry Time 5.00 hour
@Temperature 55.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Appeel® 22D843 Ethylene Acrylate
Dow Appeel® 20D867 Ethylene Acrylate
Dow Appeel® 20D855 Ethylene Acrylate
Dow Appeel® 20D828 Ethylene Acrylate
Dow Appeel® 20D784 Ethylene Acrylate

PDTA4906 / 170346

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.