Product Description: TufGel 332 is a clear, tough, moderately cross-linked silicone elastomer, which has good room temperature cure adhesion to many substrates. This material also has enhanced flame retardant properties compared to standard gels. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection. Key Features: - One to one mix ratio
- High strength
- Dispensing equipment not necessary
- Non-yellowing catalyst system
- Good adhesion to many substrates including glass, aluminum and copper with primer
Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017 |