MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Huber Pergopak® M3 Matting Agent and Carrier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Pergopak® M3 matting agent and carrier is used as a matting and effects agent for the coatings industry imparting high matting efficiency, low impact on rheology, improved scratch and abrasion resistance, improvement of adhesion and elasticity, excellent weather resistance and gloss retention. D90 17 microns.

CAS No.: 9011-05-6

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/cc
Bulk Density 0.0800 g/cc
 0.200 g/cccompressed
Solids Content >= 83 %
Oil Absorption >= 310 %310 cm3/100g
Particle Size 6.0 - 8.5 µmd50, laser diffraction
 15 - 19 µmd90, laser diffraction
 <= 36 µmd100, laser diffraction
Specific Surface Area 14 - 22 m²/gBET
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature >= 220 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.607
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 12.0 Month
 
Descriptive Properties
Functionality: Mechanical hardnessAbrasion Resistance
Functionality: Optical effectsSoft Feel Enhancer
Market/Application: Building & ConstructionPaints & Coatings
Market/Application: TransportationCoatings / Refinish Coatings

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EHUBER851 / 300957

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.