MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C37100, O50 Temper, Wire
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Light Anneal

Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Hot Formed; Good Suitability – Brazing; Fair Suitability – Butt Weld, Capacity for Being Cold Worked

Typical Uses: Decorative Knobs; Furniture Hardware; Valve Bodies for Refrigeration, Chemicals; Golf Putters; Automatic Screw Machine Parts

Applicable Specifications: Rod, Bar & Shapes – ASTM B981/B981M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.41 g/cc0.304 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 30T 4343
Tensile Strength 372 MPa54000 psi
Tensile Strength, Yield 138 MPa20000 psi
Elongation at Break 40 %40 %
Tensile Modulus 103 GPa15000 ksi
Modulus of Rigidity 38.6 GPa5600 ksi
Poissons Ratio 0.340.34Calculated
Machinability 70 %70 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000640 ohm-cm0.00000640 ohm-cm27% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.9 µm/m-°C
@Temperature 20.0 - 300 °C
11.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 9.94 W/m-K69.0 BTU-in/hr-ft²-°F
Melting Point 888 - 899 °C1630 - 1650 °F
Solidus 888 °C1630 °F
Liquidus 899 °C1650 °F
Annealing Point 427 - 593 °C800 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 621 - 788 °C1150 - 1450 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 58 - 62 %58 - 62 %
Iron, Fe <= 0.15 %<= 0.15 %
Lead, Pb 0.60 - 1.2 %0.60 - 1.2 %
Zinc, Zn 36.8 - 41.4 %36.8 - 41.4 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC37100x2 / 291875

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.