MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Chemlon® 100 XHU Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Availability: Europe; Asia Pacific; North America

Additive: Heat Stabilizer; Lubricant; UV Stabilizer

Features: General Purpose; Good Processability; Good Toughness; Heat Stabilizer; High Strength; Lubricated; UV Resistant

Uses: Appliances; Automotive Applications; Electrical/Electronic Applications

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Maximum Moisture Content 0.200.20
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 82.7 MPa12000 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Flexural Strength 114 MPa16500 psiASTM D790
Flexural Modulus 2.93 GPa425 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C190 °FUnannealed; ASTM D648
Flammability, UL94 V-2V-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 282 °C540 °F
Middle Barrel Temperature 271 °C520 °F
Front Barrel Temperature 260 °C500 °F
Nozzle Temperature 260 °C500 °F
Melt Temperature 254 °C490 °F
Mold Temperature 21.1 - 93.3 °C70.0 - 200 °F
Drying Temperature 65.6 - 82.2 °C150 - 180 °F
Injection Pressure 34.5 - 138 MPa5000 - 20000 psi
Screw Speed 60 - 120 rpm60 - 120 rpm
 
Descriptive Properties
AppearanceBlack
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0427 / 236918

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.