MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe LSS™ H12 Hot Work Tool Steel (ASTM H12)
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Hot Work Steel

Material Notes: TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel, and the tungsten content provides better temper resistance. TLS H12 hot work tool steel is a deep-hardening, air-hardening steel that exhibits minimal size change during heat treatment. It has good resistance to thermal fatigue cracking (heat checking) and excellent resistance to gross cracking and thermal shock when water cooled in service. TLS H12 hot work tool steel is recommended for hot tooling applications where maximum resistance to cracking is required. Such applications include hot punches, die casting dies, forging dies, hot shear blades, hot gripper dies, and extrusion tooling.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.68 g/cc
Density 0.277 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 53Air Cooled from 982°C, 45 minutes
 54Air Cooled from 1010°C, 45 minutes
 55Air Cooled from 1038°C, 45 minutes
Modulus of Elasticity 30000 ksi
 23000 ksi
@Temperature 538 °C
 27000 ksi
@Temperature 204 °C
Machinability 75 - 80 %1% Carbon Steel
Charpy Impact 17.0 ft-lbV-Notch; Air Cooled from 1010°C; 649°C Temper Temperature
 23.0 ft-lbV-Notch; Air Cooled from 1010°C; As Quenched
 25.0 ft-lbV-Notch; Air Cooled from 1010°C; 172°C Temper Temperature
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.7 µm/m-°C
@Temperature 27.0 - 204 °C
 14.0 µm/m-°C
@Temperature 260 - 649 °C
Thermal Conductivity 18.9 W/m-K
@Temperature 27.0 °C
 25.6 W/m-K
@Temperature 204 °C
 27.9 W/m-K
@Temperature 760 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.35 %
Chromium, Cr 5.0 %
Iron, Fe 90.65 %
Manganese, Mn 0.30 %
Molybdenum, Mo 1.4 %
Silicon, Si 1.0 %
Tungsten, W 1.3 %
Vanadium, V 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe LSS™ H10 Hot Work Tool Steel (ASTM H10)
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel
Crucible Steel CHRO-MOW® Tool Steel, AISI H12
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11
Latrobe LSS™ H11 Hot Work Tool Steel (ASTM H11)

NTIMK082 / 19429

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.