Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 90/10. It is specifically designed to give good adhesion to ceramic substrates. Applications in medical diagnostics, environmental sensor and the ’agri-food’ industries Screen Printing Equipment: semi-automatic, manual Screen Types: polyester, mesh 156-230tpi Substrate: ceramic.Information provided by Gwent Electronic Materials Ltd. |