Modern composition range listed; pewter formerly was a lead-tin alloy but lead is no longer added because of toxicity and dullness concerns. Applications include jewelry and kitchen and home decor products such as candlesticks, mugs, plates, etc. Pewter is typically cast between 315-330°C. |