MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Petropol Nypol® A3 G25 D15 HS RH PRTA011 NR467 Nylon 66, 25/15% Glass/Mineral Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes: Polyamide 6.6 black reinforced with 25% of fiberglass and 15% of mineral filled, heat stability, good set of thermal and mechanical properties. Ideal for injection molding.

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 - 1.49 g/ccASTM D792
Water Absorption 0.65 %ASTM D570
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.0070 cm/cm
@Thickness 3.18 mm
ASTM D955
Ash 38 - 42 %ISO 1172
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120
Tensile Strength at Break 147 MPaASTM D638
Tensile Strength 148 MPaASTM D638
Elongation at Break 5.0 %ASTM D638
Flexural Strength 217 MPaASTM D790
Flexural Modulus 8400 MPaASTM D790
Izod Impact, Notched 42.0 J/m
@Temperature -40.0 °C
ASTM D256
 64.0 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched 550 J/m
@Temperature -40.0 °C
ASTM D256
 640 J/m
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Strength 16.0 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 - 265 °CASTM D2217
Deflection Temperature at 0.46 MPa (66 psi) 255 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 240 °CASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 280 °CMolding
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPETROPOL110 / 313018

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.