MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay BPS 240 format 2
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: BP240 format 2 is a three-part system designed for the manufacture of car body panels with excellent surface quality at cure temperatures between 85 to 150°C (185 to 302°F). The first ply utilizes Cytec’s VTF266 sandable, paint ready surface film. The second ply is made of 400 g/m2 of Cytec’s DForm pregreg, providing fast lay-up and low print through. The third ply combines low-density syntactic core materials and structural fabric to create significant panel rigidity in a rapid laminating format. Excellent environmental performance can be expected from panels painted in Hi-Bake and Lo-Bake paint system.

Features & Benefits:

  • Flat surface
  • Paint ready form mold-no abrading or reworking
  • Readily formable-much reduced laminating time
  • Versatile cure temperatures
  • Autoclave cure
  • 12 months storage at -18°C(0°F)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature -18.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.750 hour
@Temperature 150 °C
 5.00 hour
@Temperature 85.0 °C
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCYTED130 / 180432

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.