MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Valcor® G-AZ
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: The Valcor line of fired refractory shapes, manufactured by Thermal Ceramics, has a proven track record in molten glass contact applications. The shapes are engineered to meet precise customer specifications and are individually inspected.

Features:

  • Years of proven performance in molten glass contact applications
  • Very smooth surface finish
  • Hundreds of molds in stock
  • Two compositions: G and G-AZ
  • Individual part inspection
  • Hundreds of standard molds in inventory
  • Applications:

    Consumable molten glass contact refractory shapes

  • stirrers
  • plungers
  • spouts
  • feeder tubes
  • skimmer blocks
  • Burner blocks

    Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Bulk Density 3.045 g/cc0.1100 lb/in³
    Porosity 17 %17 %Apparent
    Permeability 4.04.0ft3/hr * ft2 * in, psi
    Deformation 0.20 %0.20 %at 25 psi; 1.5 hours at 2850°F
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture  0.00965 GPa
    @Temperature 1540 °C
    1.40 ksi
    @Temperature 2800 °F
     0.0159 GPa
    @Temperature 1430 °C
    2.30 ksi
    @Temperature 2600 °F
     0.0207 GPa
    @Temperature 23.9 °C
    3.00 ksi
    @Temperature 75.0 °F
     0.0207 GPa
    @Temperature 1260 °C
    3.00 ksi
    @Temperature 2300 °F
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear 6.12 µm/m-°C
    @Temperature 20.0 °C
    3.40 µin/in-°F
    @Temperature 68.0 °F
    Melting Point 1760 °C3200 °F
    Shrinkage 0.40 %
    @Temperature 1650 °C,
    Time 18000 sec
    0.40 %
    @Temperature 3000 °F,
    Time 5.00 hour
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 64 %64 %
    Alkalis 0.20 %0.20 %
    Fe2O3 0.20 %0.20 %
    SiO2 12 %12 %
    TiO2 0.10 %0.10 %
    ZrO2 23 %23 %
     
    Descriptive Properties
    MgO Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM164 / 2484

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.