MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Go Yen Chemical GY-MG40 Inorganic Flame Retardant for Rubber
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • Natural and synthetic rubber: EPDM, NR, CR, EVA, SBR, NBR, IIR, BR
  • various kinds of tyre
  • Related flame retardant constructional materials, roofing, waterproof tapes & elastomers
Applications:
  • GY- MG40 provides excellent disperse ability
  • Can be applied in different kinds of rubbery industry field
  • GY- MG40 process by special treatment of Stearic acid
  • High Thermal temperature
  • GY- MG40 won excellent flame retardant ability
  • Good smoke suppression ability to those product and forming item
  • Applied in the field of plastic and rubbery for its permanent effective.
  • Other special application

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.352 g/cc0.0127 lb/in³Loose
 0.577 g/cc0.0208 lb/in³Tapped
Brightness 95.5 %95.5 %Whiteness
Particle Size 2.0 - 5.0 µm2.0 - 5.0 µm
Particle Mesh Size 325 Mesh325 Mesh>99%, Sieve
Specific Surface Area 7.0 - 13 m²/g7.0 - 13 m²/g
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) <= 30 %<= 30 %
 
Descriptive Properties
AppearanceFine powder
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN461 / 266769

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.