MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Firecrete STD Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Chamotte raw material base. Hydraulic bond. A high strength, general purpose concrete for casting and gunning application to 1400°C/2550°F. It is especially effective for boilers, door lining, furnace lining, car tops and monolithic furnaces.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.09 g/cc0.0755 lb/in³dried to 110°C
Grain Size <= 5000 µm<= 5000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 35.3 MPa5120 psiCold Crushing Strength, MST
 22.5 MPa
@Treatment Temp. 1000 °C
3260 psi
@Treatment Temp. 1830 °F
Cold Crushing Strength
 27.4 MPa
@Treatment Temp. 815 °C
3970 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 36.3 MPa
@Treatment Temp. 110 °C
5260 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.590 W/m-K
@Temperature 400 °C
4.09 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.640 W/m-K
@Temperature 600 °C
4.44 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 0.710 W/m-K
@Temperature 800 °C
4.93 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 0.810 W/m-K
@Temperature 1000 °C
5.62 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 0.930 W/m-K
@Temperature 1200 °C
6.45 BTU-in/hr-ft²-°F
@Temperature 2190 °F
Maximum Service Temperature, Air <= 1400 °C<= 2550 °F
Shrinkage 0.50 %0.50 %MST
 0.20 %
@Treatment Temp. 815 °C
0.20 %
@Treatment Temp. 1500 °F
 0.20 %
@Treatment Temp. 1000 °C
0.20 %
@Treatment Temp. 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 41.6 %41.6 %
CaO 10.7 %10.7 %
Fe2O3 5.2 %5.2 %
K2O+Na2O 0.30 %0.30 %Na2O + K2O
SiO2 40 %40 %
TiO2 1.8 %1.8 %
 
Descriptive Properties
Net Material Required (kg/m³)1970
Water Addition14% by weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6386 / 203170

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.