MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CHT Group EP MAP-Z 10 EPI Engineered Polymers Aliphatic Prepolymer
Categories: Fluid

Material Notes: EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are available. EP MAP Z has been designed for use as a primer for steel to prevent corrosion. Colors may be added due to its aliphatic nature. A clear top-coat of EP RAP60M may be used over EP MAP Z. Solvents such as xylene, MEK, or butyl acetate may be used to cut EP MAP Z to improve sprayability. EP Map-Z 10 contains 10 % NCO

Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc
@Temperature 25.0 °C
1.50 g/cc
@Temperature 77.0 °F
Viscosity 2150 cP2150 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point -23.0 °C-9.40 °F
Flash Point 213 °C415 °FPMCC
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PACC093 / 22220

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.