MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Bynel® 41E850 Anhydride Modified LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextrusion equipment designed+F47 to process polyethylene resins.

Physical properties of BYNEL Series 4100 resins are typical of linear low-density polyethylene resins with similar density and melt index values. Use of these adhesive resins in coextruded PE/barrier structures offers improved thermal resistance over that of ethylene vinyl acetate-based adhesive resins.

BYNEL 4100 series resins adhere to a variety of materials. They are most often used to adhere to EVOH, polyamide, PE and ethylene copolymers. Series 4100 resins can be used in coextrusion processes including:

  • blown film
  • cast film/sheet
  • blow molding
  • melt and solid phase thermoforming
  • sheet and tubing

LLDPE resins are known for their temperature resistance, clarity and toughness. These physical properties make the 4100 series resins work well in applications such as:

  • boil-in-bag structures
  • blow molded containers in which drop strength is important
  • bag-in-box films
  • film where LLDPE is the heat seal layer

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792, ISO 1183
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 103 °CFreezing Point; ASTM D3418
 120 °CASTM D3418, ISO 3146
Vicat Softening Point 88.0 °CASTM D1525, ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 260 °C
Feed Temperature 160 °CCoExtrusion with EVOH Processing
 160 °CCoExtrusion with Nylon Processing
Zone 2 185 °CCoExtrusion with EVOH Processing
 185 °CCoExtrusion with Nylon Processing
Zone 3 235 °CCoExtrusion with EVOH Processing
 235 °CCoExtrusion with Nylon Processing
Zone 4 235 °CCoExtrusion with EVOH Processing
 260 °CCoExtrusion with Nylon Processing
Zone 5 235 °CCoExtrusion with EVOH Processing
 260 °CCoExtrusion with Nylon Processing
Adapter Temperature 235 °CCoExtrusion with EVOH Processing
 260 °CCoExtrusion with Nylon Processing
Die Temperature 235 °CCoExtrusion with EVOH Processing
 260 °CCoExtrusion with Nylon Processing
Melt Temperature 210 - 235 °CCoExtrusion with EVOH Processing
 <= 260 °CCoExtrusion with Nylon Processing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Bynel® 41E865 Anhydride Modified LLDPE
Mitsui ADMER® NF548A PE Type Polyolefin
Dow Bynel® 42E703 Adhesive Resin
Mitsui ADMER® NF908A PE Type Polyolefin
Dow Bynel® 21E787 Anhydride Modified Ethylene Acrylate

PDTA4928 / 170368

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.