MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot CAB-O-SIL® ELM-150 Fumed Silica
Categories: Other Engineering Material

Material Notes: Product highlights: CAB-O-SIL ELM-150 fumed silica is a high purity fumed silica with a nominal nitrogen BET surface area of 160 m2/g. The product is designed for use in dispersion and slurry formulations used to polish silicon wafers/semiconductors for IC fabrication. CAB-O-SIL ELM-150 fumed silica is characterized by:
  • High chemical purity
  • Narrow surface area range
  • Narrow particle size distribution
  • Low lot to lot variation
  • High product consistency
Key application: Chemical Mechanical Planarization (CMP): Since the mid-1990s, the use of CMP has grown rapidly in semiconductor manufacturing. As a polishing technique, CMP facilitates smooth, clean, and planar surfaces by utilizing carefully formulated and controlled dispersions of fumed metal oxides, and other particles, in conjunction with specially designed equipment and polishing pads. The polishing process precisely removes excess build-up of dielectric insulation (oxide) and tungsten (plugs and vias <500 nm) that occur during the semiconductor manufacturing process. Specifically, formulating fumed silica dispersions and slurries with CAB-O-SIL ELM-150 product enables planarity and erosion control with high removal rate during tungsten CMP processes.

Performance benefits :Dispersions and slurries designed for the precise and highly controlled CMP process require fumed silicas that are specifically engineered and consistently manufactured to enable CMP formulations to:

  • Optimize the polishing/removal rate
  • Deliver planarity and uniformity across the silicon wafer
  • Minimize polishing defects (micro-scratching/LPCs) and erosion
  • Minimize contaminant metals
  • Deliver uniform and consistent lot-to-lot performance
  • Lower Cost of Ownership along the fabrication channel

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Surface Area 160 m²/g
 
Descriptive Properties
Product FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT078 / 315813

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.