MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec Rocar® SiF Silicon Carbide, SiSiC
Categories: Ceramic; Carbide

Material Notes: Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden changes in temperature, excellent anti-friction properties, and higher heat conductivity over steel. The various types of Rocar include sintered and silicon infiltrated silicon carbide. In SiSiC, the pore cavities are filled with metallic silicon. Since shrinkage during firing is minimal, complex components can be produced with low tolerances. It maximum application temperature is 1350°C. However, it is not suitable for use in highly alkaline media because of its content of metallic silicon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.07 g/ccDIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 %DIN EN 623-2 / ASTM-C373
Porosity 0.00 %Closed (approximate)
Permeability 0.00Gas
Weibull Modulus >= 14DINV ENV 843-5
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1200HV 0.2; Si; DINV ENV 843-4
 2700HV 0.2; SiC; DINV ENV 843-4
Tensile Strength at Break 350 MPaACMA Test #4 / DIN EN 843-1
Tensile Modulus 395 GPaYoung's; DINV ENV 843-2 / ASTM-F417
Flexural Strength 350 MPa
@Temperature 20.0 °C
DIN EN 843-1
 350 MPa
@Temperature 1000 °C
DIN EN 820-1
Compressive Strength 3500 MPaASTM C-773-88 / DIN 51067T1
Poissons Ratio 0.17DINV ENV 843-2
Fracture Toughness 4.00 MPa-m½DIN 51109
Shear Modulus 169 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.0 ohm-cm
@Temperature 20.0 °C
IEC 672-1
 100 ohm-cm
@Temperature 400 °C
IEC 672-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.80 µm/m-°C
@Temperature 20.0 - 200 °C
DIN EN 821-1
 4.30 µm/m-°C
@Temperature 20.0 - 400 °C
DIN EN 821-1
 4.50 µm/m-°C
@Temperature 20.0 - 600 °C
DIN EN 821-1
 4.90 µm/m-°C
@Temperature 20.0 - 1000 °C
DIN EN 821-1
Specific Heat Capacity 0.700 J/g-°C
@Temperature 100 - 200 °C
DINV ENV 821-3
 1.30 J/g-°C
@Temperature 1000 °C
DINV ENV 821-3
Thermal Conductivity 40.0 W/m-K
@Temperature 1000 °C
DIN EN 821-2
 120 W/m-K
@Temperature 20.0 - 100 °C
DIN EN 821-2 / ASTM-C408
Maximum Service Temperature, Air 1350 °C
Maximum Service Temperature, Inert 1350 °C
 
Descriptive Properties
ColorBlack
Ra = Arithmetic Mean Roughness Value (µm)Profilometer (0.8 mm Cutoff)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, Reaction-Bonded, SiSiC
CeramTec Rocar® SiG Silicon Carbide, SiSiC
CeramTec Rocar® ST Silicon Carbide, SSiC
CeramTec Rocar® S Silicon Carbide, SSiC
Morgan Advanced Ceramics CVD Silicon Carbide

CCERA941 / 107541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.