MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wefapress Nylatec Slide Pro
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Withstands temperatures of >100°C for long periods of time, high pressure resistance, High wear resistance, Excellent impact resistance, Self-lubricating.

Applications: Drive element, Guide rails, Sliding profiles, slide bearings, slide rails, Guide and track rollers, Deflection pulleys. Industries: Conveyor systems and automation, Mechanical and plant engineering.

Information provided by Wefapress.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDIN 53479
Moisture Absorption <= 2.30 %
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 155 MPa
@Time 30.0 sec
DIN ISO 2039 Teil 1
Tensile Strength >= 16.0 MPaDIN 53455
Tensile Strength, Ultimate 125 MPaDIN 53455
Elongation at Break 40 %DIN ISO / R 527
Modulus of Elasticity 3.10 GPaDIN 53457
Charpy Impact, Notched >= 4.00 kJ/m²DIN 53457
Coefficient of Friction <= 0.15
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Strength 50.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear <= 70.0 µm/m-°CDIN ISO 11359
Specific Heat Capacity 1.70 J/g-°C
Thermal Conductivity 0.230 W/m-K
Melting Point 215 °CDTA
Maximum Service Temperature, Air 105 °CContinuous Application Temp.
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWEFA949 / 243154

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.