Temper: As Centrifugal Cast Fabrication Properties: Excellent Suitability – Soldering; Good Suitability - Brazing; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding Typical uses: Nuts; Bearings; Bushings; Fittings; Gears; Piston Rings; Pump Impellers; Steam Castings Applicable Specifications: As Centrifugal Cast – Castings ASTM B427; As Sand Cast – Castings ASTM B427; Ingot - ASTM B30 |