MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics Formolene® 6530N Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: Formolene® 6530N is a high impact, copolymer polypropylene. It was specifically developed to meet the OEM requirements of automotive interior door panels used for above shoulder applications. Material has been approved under Renault-Nissan AS3. This material is free of animal-derived content.

Availability: North America

Features: Copolymer; High Impact Resistance; No Animal Derived Components

Uses: Automotive Interior Parts

Automotive Specifications: RENAULT AS3

Form: Pellets

Processing Method: Injection Molding

Information provided by Formosa Plastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.0 MPa2760 psiInjection Molded; ISO 527-2/50
Elongation at Yield 5.0 %5.0 %Injection Molded; ISO 527-2/50
Flexural Modulus 0.972 GPa141 ksi1% Secant, Injection Molded, 0.051 in/min; ISO 178
Izod Impact, Notched (ISO)  7.98 kJ/m²
@Temperature -40.0 °C
3.80 ft-lb/in²
@Temperature -40.0 °F
Injection Molded; ISO 180
 9.45 kJ/m²
@Temperature -30.0 °C
4.50 ft-lb/in²
@Temperature -22.0 °F
Injection Molded; ISO 180
 42.0 kJ/m²
@Temperature 22.8 °C
20.0 ft-lb/in²
@Temperature 73.0 °F
Injection Molded; ISO 180
Charpy Impact, Notched  0.693 J/cm²
@Temperature -40.0 °C
3.30 ft-lb/in²
@Temperature -40.0 °F
Injection Molded; ISO 179
 0.798 J/cm²
@Temperature -30.0 °C
3.80 ft-lb/in²
@Temperature -22.0 °F
Injection Molded; ISO 179
 5.04 J/cm²
@Temperature 22.8 °C
24.0 ft-lb/in²
@Temperature 73.0 °F
Injection Molded; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C189 °FUnannealed; ISO 75-2/Be
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C120 °FUnannealed; ISO 75-2/Ae

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFPCR748 / 311441

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.