MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Lehvoss LUVOCOM® 1-8843 Polyamide 66 with glass fiber, thermally conductive modified, heat stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Properties/attributes include: Strong, stiff parts. Emergency-running capability.

Automotive industry, textile- and office machinery, apparatus- and precision engineering. Typical uses include: Coil formers, duty parts in plugs and switches, body parts.

Processing: During processing the moisture level should not exceed 0.1%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. Excessively high predrying temperatures may cause discoloration. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.57 g/cc1.57 g/ccISO 1183
Moisture Absorption <= 1.00 %
@Temperature 23.0 °C,
Time 86400 sec
<= 1.00 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 145 MPa21000 psiISO 527-2
Elongation at Break 2.3 %2.3 %ISO 527-2
Modulus of Elasticity 10.0 GPa1450 ksiISO 527-2
Flexural Strength 210 MPa30500 psiISO 178
Flexural Modulus 9.00 GPa1310 ksiISO 178
Flexural Strain at Break 3.2 %3.2 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 4.90 J/cm²
@Temperature 23.0 °C
23.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+11 ohm-cm>= 1.00e+11 ohm-cmIEC 60167
Surface Resistance >= 1.00e+11 ohm>= 1.00e+11 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.10 W/m-K14.6 BTU-in/hr-ft²-°FHOT-DISK || 60x60x3 mm
Maximum Service Temperature, Air 120 °C248 °FContinuous; UL 746B
 160 °C320 °FShort Term
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 300 °C536 - 572 °F
Zone 1 290 - 310 °C554 - 590 °F
Zone 2 290 - 310 °C554 - 590 °F
Zone 3 290 - 310 °C554 - 590 °F
Melt Temperature 290 °C554 °F
Mold Temperature 90.0 - 120 °C194 - 248 °F
Drying Temperature  75.0 °C
@Time 21600 - 57600 sec
167 °F
@Time 6.00 - 16.0 hour
Dehumidifying dryer
 105 °C
@Time 14400 - 21600 sec
221 °F
@Time 4.00 - 6.00 hour
Vacuum Dryer
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Colordark grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUU8897 / 193856

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.