MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Matexcel NAT-197 Curdlan
Categories: Other Engineering Material

Material Notes: Gel. Strength: 450g/cm2 min. pH(1% solution): 6.0-7.5 Loss on drying: <10/% Ash: <6.0% Total Nitrogen: <1.5%

Application: Curdlan is a kind of fermentation product. Under normal temperature, Curdlan could swell after absorbing water, insoluble in water and alcohol. Curdlan is able to dissolve in alkalinous solution with pH above 11. After heating, Curdlan could absorb 50 times water to form gels. As food additive, Curdlan could help to improve the moisture containing ability, Q- characteristics, stability, thickening ability, which allow to enhance foods processing ability and the mouth feel. Curdlan is widely applied in meat products, meat ball products, tofu products, Bionic vegetarian diet and bakery products.

Morphology: White of off-white powder

Uses: Gelling in low temperature: when Curdlan solution is heated up to 55-65 Celcius Degrees, then cooling down to 40 centigrade below, heat-reversible gels would form, heating again could help to form high temperature gels. Gelling in high temperature: when Curdlan solution is heated up to more than 80 centigrade, Curdlan could help to form high gel strength heat-stable gels. This gel is heatirreversible and even after being iced and melted, the gel. Strength is still stable. Main characteristics: gelling, heat-irreversible, elastic Q-Characteristics, Water Absorb, Heat Stable, Acid and alkalinous Stability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Purity>80%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1255 / 299886

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.