MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Dyneon™ CC607 PTFE 35% Fiberglass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.

Data provided by Dyneon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.23 g/cc0.0806 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858value after 15 sec; ASTM D2240
 6363initial value; ASTM D2240
Tensile Strength, Ultimate 13.1 MPa1900 psiASTM D4745
Elongation at Break 180 %180 %ASTM D4894
Flexural Yield Strength <= 18.0 MPa<= 2610 psiASTM D790
Compressive Yield Strength 7.80 MPa1130 psiASTM D695
Compressive Modulus 0.430 GPa62.4 ksiASTM D695
Coefficient of Friction, Dynamic 0.360.36ASTM D3702
Coefficient of Friction, Static 0.270.27ASTM D3702
K (wear) Factor 142 x 10-8 mm³/N-M70.6 x 10-10 in³-min/ft-lb-hrat 5000 psi - fpm PV; ASTM D3702
 
Thermal PropertiesMetricEnglishComments
CTE, linear 162 µm/m-°C
@Temperature 20.0 °C
90.0 µin/in-°F
@Temperature 68.0 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ CC604 PTFE, 20% Fiberglass Filled
AGC Fluon® FC 405 PTFE, 25% Glass Fiber Filled
AGC FC 105 PTFE, 25% Glass Fiber
AGC Fluon® FP-EF-105 PTFE, 25% Glass Filled
AGC Fluon® RB1025S 25% Glass Fiber, PTFE Filled Compound

PDYM68 / 34680

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.