MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Geniosil® GF 56 Silane
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Empirical formula: C8H18O3Si

CAS No.: 78-08-0

Properties: The use of GENIOSIL® GF 56 as a co-monomer in polymers results in binders which, among other advantages, exhibit much improved wet scrub resistance and abrasion resistance thanks to crosslinking and better adhesion to the substrate. Silane-modified thermoplastics obtained by grafting with GENIOSIL® GF 56 can be processed further using standard techniques. On exposure to moisture (e.g. water bath, climatic chamber), the silyl groups condense (ethanol is released) and function as crosslinking and/or adhesion points. By treating fillers with GENIOSIL® GF 56, mineral filled polymers can be obtained which exhibit improved mechanical and electrical properties. In addition, the particles are rendered strongly water repellent, which results in improved filler dispersibility and thus facilitates processing. Organic surface coatings will adhere more strongly to inorganic substrates that have been treated with GENIOSIL® GF 56. As a result, these coatings demonstrate markedly greater scratch resistance and resistance to chemicals.

Special features: GENIOSIL® GF 56 is an alkoxy vinyl silane. It´s a clear, colorless liquid with a characteristically aromatic odor.It hydrolyzes in the presence of moisture (ethanol is released) to form silanols, which can then react with themselves to produce siloxanes .As a bifunctional molecule, GENIOSIL® GF 56 is able to function as a molecular bridge between organic and inorganic substrates.

Application: GENIOSIL® GF 56 is used in the production of silane modified polymers that serve as binders in paints and adhesives. GENIOSIL® GF 56 is also used in the manufacture of pipes and cables made of silane crosslinked polyethylene (PE-Xb). In addition, GENIOSIL® GF 56 serves as an adhesion promoter in primers and coatings, and is used in the production of organically modified fillers for cable insulation.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccDIN 51757
Molecular Weight 190.3 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point >= 158 °C
@Pressure 0.1013 MPa
Flash Point 37.0 °CISO 3679
Ignition Temperature 265 °Cliquids; DIN 51794
 
Descriptive Properties
Content<10 mg/kgHydrolyzable chloride (as HCl)
Purity>98%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9311 / 204840

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.