MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dysprosium, Dy
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.54 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 162.501995
Atomic Number 66
X-ray Absorption Edge 0.23046 ÅK
 1.36926 ÅLI
 1.44357 ÅLII
 1.59025 ÅLIII
Electronegativity 1.22Pauling
Ionic Radius 0.908 ÅCrystal Ionic Radius for Valence +3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 44
Tensile Strength, Ultimate 246 MPa
Tensile Strength, Yield 225 MPa
Elongation at Break 30 %
Tensile Modulus 61.4 GPa
Bulk Modulus 40.5 GPa
Poissons Ratio 0.237
Shear Modulus 24.7 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000925 ohm-cm
Magnetic Susceptibility 0.000614cgs/g
Curie Temperature -184 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 106 J/g
CTE, linear 9.90 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.175 J/g-°C
Thermal Conductivity 10.0 W/m-K
Melting Point 1409 °C
Boiling Point 2567 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.297
@Wavelength >=645 nm,
Temperature 1425 °C
Liquid
 
Component Elements PropertiesOriginal ValueComments
Dysprosium, Dy 100 %
 
Descriptive Properties
CAS Number7429-91-6

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Americium, Am
Chromium, Cr; Recrystallized
Silver, Ag
Copper, Cu; Cold-Worked
Erbium, Er

AMEDy00 / 31

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.