MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATG s.r.l. BR Polybutadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 90
Tensile Strength, Ultimate 7.00 - 18.0 MPa
Elongation at Break 120 - 800 %
Rebound 30 - 70 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °C
Minimum Service Temperature, Air -50.0 °C
 
Descriptive Properties
Abrasion Resistancehigh
Chemical Resistance to Animal and Vegetable Oils and Greasesnone
Chemical Resistance to Aromatic Hydrocarbonsnone
Chemical Resistance to Chloride Solventsnone
Chemical Resistance to Distilled Watermedium
Chemical Resistance to Ketonesmedium
Chemical Resistance to Maximum Concentrated Alkalis (at 50°C)medium
Chemical Resistance to Medium-High Concentrated Acids (at 50°C)low
Chemical Resistance to Mineral Oils and Aliphatic Hydrocarbonsnone
Compression set at 100°Cmedium
Impermeability at gas (Oxygen and Nitrogen)low
Resistance to Flamenone
Resistance to Heat Aginglow
Resistance to Low Temperatureshigh
Resistance to Ozone and Weatheringlow
Tear Strengthmedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polybutadiene Rubber (BR)
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Dow Buna® cis 132 High-cis polybutadiene rubber (nickel catalyzed) for tires and rubber articles
ATG s.r.l. IR Synthetic Polyisoprene
Dow SE BCP 817 Stereospecific high cis-1,4 Polybutadiene (BR)

PATG004 / 79369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.