MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kraiburg TPE HIPEX® HX6ICN Thermoplastic Elastomer, High Performance  (Unverified Data**)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: The HTR/OR Series is recommended for applications requiring high temperature and oil resistance.

Typical applications:

  • Closures
  • Fastenings
  • Flexible Connections
  • Seals
Material advantages:
  • Excellent heat resistance up to 150 °C
  • Excellent resistance against motor and gearbox oil
  • For injection molding
  • Recyclable
Processing Method: Injection Molding

Information provided by Kraiburg TPE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³DIN EN ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858DIN ISO 7619
Tensile Strength 5.00 MPa725 psiDIN 53504/ISO 37
Elongation at Break 300 %300 %DIN 53504/ISO 37
Tear Strength 13.5 kN/m77.0 pliDIN ISO 34-1
Compression Set  30 %
@Temperature 25.0 °C,
Time 259000 sec
30 %
@Temperature 77.0 °F,
Time 72.0 hour
DIN ISO 815
 54 %
@Temperature 70.0 °C,
Time 86400 sec
54 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815
 58 %
@Temperature 100 °C,
Time 86400 sec
58 %
@Temperature 212 °F,
Time 24.0 hour
DIN ISO 815
 64 %
@Temperature 120 °C,
Time 86400 sec
64 %
@Temperature 248 °F,
Time 24.0 hour
DIN ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 °C410 °F
Middle Barrel Temperature 220 °C428 °F
Front Barrel Temperature 230 °C446 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 105 °C
@Time 7200 sec
221 °F
@Time 2.00 hour
Injection Pressure 130.00 - 200.0 MPa18855 - 29010 psi
Back Pressure 1.97 - 4.90 MPa285 - 710 psi
 
Descriptive Properties
ColorNatural
Hot Runner180-220°CThe runner should be empty after a maximum of 2 - 3 shots.

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry)
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin
MRC Polymers NAXALOY™ 780-11G PC + PBT Blend
MRC Polymers NAXALOY 740 Polycarbonate/ASA blend
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin

PKRAIA8741 / 171399

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.