MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotchcal™ 8000-13 Graphic Film
Categories: Polymer; Film

Material Notes: This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by commercial and industrial graphics, providing outstanding long-term durability for fleet, sign and railroad graphics. It is available in several colors with a paper or layflat liner.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milwithout adhesive
 76.2 - 102 microns3.00 - 4.00 milwith adhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 17.2 MPa>= 2490 psi
Peel Strength 0.701 kN/m4.00 pliAdhesion to ABS
 0.701 kN/m4.00 pliAdhesion to Acrylic enamel
 0.701 kN/m4.00 pliAdhesion to Fruehauf pre-painted panel
 0.877 kN/m5.00 pliAdhesion to Chrome
 1.05 kN/m6.00 pliAdhesion to Aluminum, anodized
 1.05 kN/m6.00 pliAdhesion to Aluminum, etched
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 4.00 °C>= 39.2 °FApplication Temperature
 
Descriptive Properties
AppearanceTomato red

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35036 / 169783

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.