MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Superior Flux Superior No. 612 High Temperature Brazing Paste Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Specially formulated high temperature brazing flux.
  • For use on ferrous alloys, stainless steels, carbides, and other specialty alloys.
  • Residues are water-soluble.
Description: Superior No. 612 is a high temperature brazing paste flux that is active and protective to 1,205ºC/2,200ºF. It was specially formulated to meet the process requirements of high-temperature filler alloys, such as Manganese containing alloys, low-fuming Bronze (CDA 681) and nickel-silver (CDA 773). It is recommended for joining carbide to stainless steel, ferrous alloys, and other alloys requiring high temperature brazing.

Applications: Superior No. 612 is a boron-modified brazing flux used with high-temperature alloys for manufacturing a wide variety of products including; carbides, stainless steel, large steel parts, or processes requiring a long heating cycle.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/cc
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 760 - 1150 °C1400 - 2100 °FActive Range
 
Processing PropertiesMetricEnglishComments
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
ColorWhite
FormCreamy Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSFLUX084 / 185768

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.