MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
JSC SKI-3S Synthetic rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: SKI-3S cis-isoprene synthetic rubber is cis-1,4-polyisoprene obtained by polymerization of isoprene in solution using stereo specific catalyst based on titanium. The rubber is stabilized by mixture of two non-staining antioxidants. Content of cis-1,4-units, min: 96 %.REACH registered; KKDIK, K-REACH, DUIN pre-registered.

CAS: #9003-31-0

Application: for manufacture of auto tyres for lining of side-frames as well as colored bicycle and motorcycle tyres, and also in manufacture of colored rubber goods, non-colored industrial rubber goods used in manufacturing industry (rubber hoses, tubes, shoe soles). Rubber should not contain any foreign impurities and must meet the following requirements

Appearance: briquettes (bales)

Color: from white to light-milky

Information provided by JSC, Synthez-Kauchuk

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 - 0.920 g/cc
Volatiles <= 0.80 %
@Time 3600 sec
ASTM D5668
Mooney Viscosity <= 5.0spread within a batch
 72 - 88
@Temperature 100 °C
ML 1+4; ASTM D 1646
Ash <= 0.35 %ASTM D 5667
Storage Temperature <= 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Content0.15-0.4%antioxidants: Agidol-1 (???)
 0.4-0.2%antioxidants: Tris (2,4-di-tert-butylphenyl) phosphite
 0.5-1.5%Stearic acid
Rheometric Properties11-15 dNmMH, ASTM D 5289
 1-2 dNmML, ASTM D 5289
 2.3-3.5 mints1, ASTM D 5289
 3.9-5.2 mint50, ASTM D 5289
 6.8-8.4 mint90, ASTM D 5289

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSC023 / 317843

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.