MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kostat 5000 TAB Spacer Tapes PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: 5000 TAB Spacer Tapes, uniquely formulated and manufactured by KOSTAT, are made of various thermoplastic substrates with ICP (Inherently Conductive Polymer) coating technology. This class of materials has distinctive advantages in ESD and cleanliness performances in comparison to other materials based on hygroscopic antistats and conductive fillers. Also, this product exhibits superior transparency and clarity that will provide a convenience of being able to inspect the components with the naked vision.

Special Features:

  • Superior Permanent Static Dissipation
  • Humidity Insensitivity
  • Low Particle Generation
  • Superior Transparency and Clarity
  • Excellent Chemical Resistance with Environmentally Friendly Materials

Applications:

  • Flexible PCB Films
  • Driver IC Films for TCP, COF and COG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPaASTM D638
Flexural Strength 70.0 MPaASTM D790
Flexural Modulus 1.95 GPaASTM D790
Izod Impact, Notched 97.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1e+05 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 158 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 85 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKOSTAT19 / 49054

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.