MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ChevronTexaco Ulti-Plex® NLGI 1 Greases EP
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Features

Chevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.

They are manufactured using selected highly refined, high viscosity base oils, a lithium complex thickener, rust and oxidation inhibitors, and extreme pressure and tackiness additives. They are purple in color and stringy in texture.

The lithium complex thickener in Chevron Ulti-Plex Greases EP elevates the dropping point to approximately 265°C (510°F).

Applications

These greases are recommended for applications operating in the temperature range of -26°C to 177°C (-15°F to 350°F). Chevron Ulti-Plex Greases EP are ideal for a wide variety of industrial and automotive applications across several industries, including:

  • Paper and Forest Products — These lubricants are superior for severe service applications such as: sludge press bearings, lime kilns, pumps, woodyard heavy equipment, Doctor oscillator bearings, felt roll bearings, pulp refiner bearings, rope sheaves, and exhaust fan bearings.
  • Mining — Applications appropriate for these greases include: pins and bushings on buckets and loaders, shaker screens, crushers, and conveyors.Off-Road Construction — These greases display superior water washout resistance properties in wet, off-road environments, as well as excellent shock load protection.
  • Steel — Steel mill applications often involve extremely high temperatures. The excellent structural stability of these greases makes them appropriate in these situations. Extreme pressure properties and resistance to water washout are also key in the steel mill environment.
  • Marine — The rust and corrosion inhibition properties of Chevron Ulti-Plex Greases EP make them ideal for use in marine equipment exposed to severe corrosion environments. Examples include deck cranes and offshore drilling equipment.

Key Words: CPS Number: 250186; MSDS Number: 6701
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 80Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1636 SUS
Saybolt Viscosity at 210°F 106 SUS
Kinematic Viscosity at 40°C (104°F) 305 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 21 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 400 kgWeld Point
Four Ball Wear 0.380 mm
Penetration 325Worked
Penetration P(0), 1/10 mm 300
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -26.0 °C
Flash Point 274 °CASTM D92
Dropping Point 265 °C
 
Descriptive Properties
ColorPurple
Corrosion, Copper Strip Test 3h2A
Lincoln Ventmeter, psig at 30 s, at 0°F975
Lincoln Ventmeter, psig at 30 s, at 30°F250
TextureStringy
Thickener, % / type7 / Lithium Complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV275 / 74890

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.