MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Parson Adhesives PARTITE® 9392 Acrylic Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: PARTITE 9392 a no-mixing, high viscosity combined with a very fast cure speed structural adhesive for wide variety of industrial assembly applications, which require very fast assembly. It bonds wide range of materials with the use of Activator 1387 or 1380.

FEATURE:

  • Adhesive is applied to one surface and Activator to the other; press together and fixing is achieved within few minutes.
  • Provide tough durable bond with excellent impact and vibration resistance.
APPLICATIONS:
  • Ideal for bonding Metals, Ferrite, Plated Metals, Magnet, Wood, etc.
  • Particularly suited to DC motor assembly, magnet bonding and bonding of pre-coated sheet metal. Ideal for automated assembly lines.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/cc
Brookfield Viscosity 50000 - 75000 cP50000 - 75000 cPRVT
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 17.9 MPa>= 2600 psiISO 37
Elongation at Break 125 %125 %ISO 37
Tensile Modulus >= 0.138 GPa>= 20.0 ksiASTM D638
Shear Strength >= 15.00 MPa>= 2175 psiSteel to Steel, grit blasted; ISO 4587
Peel Strength >= 2.63 kN/m>= 15.0 pliISO 11339
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.54.5DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FASTM D696
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
Flash Point >= 92.0 °C>= 198 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1.00 - 1.50 min0.0167 - 0.0250 hourSpeed
 1440 min24.0 hourFull
 
Descriptive Properties
ColorClear Amber Liquid
CompositionUrethane Methacrylate
Gap Filling0.05-0.5 mmCured
Initial Strength Retained (%)100Motor Oil for 500 hrs at 125°C
 100Motor Oil for 1000 hrs at 125°C
 55Ethanol for 1000 hrs at 22°C
 55Water/Glycol for 1000 hrs at 87°C
 60Water/Glycol for 500 hrs at 87°C
 60Acetone for 1000 hrs at 22°C
 65Ethanol for 500 hrs at 22°C
 65Acetone for 500 hrs at 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPARSN089 / 186532

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.