MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® B3WG7 BK00564 35% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: Ultramid B3WG7 BK00564 is a 35% glass fiber reinforced, pigmented black, injection molding PA6 grade for highly rigid, dimensionally stable components which are resistant to high temperature aging and have improved retention of properties in a hot water environment.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Linear Mold Shrinkage 0.0030 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 188 MPa5mm/min; ISO 527
Elongation at Break 2.9 %5mm/min; ISO 527
Tensile Modulus 12600 MPa1mm/min; ISO 527
Flexural Modulus 9720 MPaISO Data
Izod Impact, Notched (ISO) 11.2 kJ/m²ISO Test
Charpy Impact, Notched 0.920 J/cm²ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10 K/min
Deflection Temperature at 1.8 MPa (264 psi) 215 °CISO 75
 
Descriptive Properties
ColorBK00564
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Radici Radilon® S RV350 (dry) Nylon 6
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned)
Radici Radilon® S RV350 (cond.) Nylon 6
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Overview of materials for Nylon 66, 40% Glass Fiber Filled

PBASF9336 / 85100

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.