MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
3D Systems LaserForm® Ni625 (A), AFTER STRESS RELIEF Nickel Super Alloy
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Ni625 fine-tuned for use with ProX® DMP 320 metal printer producing industrial parts with high heat resistance, high strength and high corrosion resistance. LaserForm Ni626

Ni625 is known for its combination of high strength and excellent corrosion resistance. LaserForm Ni625 (A) is the ideal material for industries where these two strengths need to come together: chemical, marine, aerospace and nuclear industry. Applications include: reaction vessels, tubing, heat exchangers, valves, engine exhaust systems, turbine seals, propeller blades, submarine fittings, propulsion motors, reactor core and control-rod components in nuclear water reactors.

Classification: The chemical composition of LaserForm Ni625 (A) corresponds to ASTM F3056, UNS N06625, Werkstoff Nr. 2.4856, DIN NiCr22Mo9Nb and AMS 5666.

Information provided by 3D Systems

Key Words: UNS N06625
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.44 g/ccAbsolute theoretical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 28 - 35ASTM E18
Tensile Strength, Ultimate 1020 - 1080 MPaVertical direction - Z; ASTM E8M
 1050 - 1170 MPaHorizontal direction - XY; ASTM E8M
Tensile Strength, Yield 660 - 740 MPaRp0.2%, Vertical direction - Z; ASTM E8M
 690 - 810 MPaRp0.2%, Horizontal direction - XY; ASTM E8M
Elongation at Break 16 - 22 %Horizontal direction - XY; ASTM E8M
 20 - 26 %Vertical direction - Z; ASTM E8M
Reduction of Area 24 - 28 %Vertical direction - Z; ASTM E8M
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.8 µm/m-°C
@Temperature 93.0 °C
 14.0 µm/m-°C
@Temperature 538 °C
 15.8 µm/m-°C
@Temperature 871 °C
Thermal Conductivity 9.80 W/m-K
Melting Point 1290 - 1350 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.40 %
Chromium, Cr 20 - 23 %
Cobalt, Co <= 1.0 %
Copper, Cu <= 0.50 %
Iron, Fe <= 5.0 %
Manganese, Mn <= 0.50 %
Molybdenum, Mo 8.0 - 10 %
Nickel, Ni >= 58 %
Niobium, Nb (Columbium, Cb) 3.15 - 4.15 %
Tantalum, Ta <= 0.050 %
Titanium, Ti <= 0.40 %
 
Descriptive Properties
Surface Roughness1-4µmHorizontal direction (XY), SAND BLASTED
 4-7µmHorizontal direction (XY), AS BUILT
 4-7µmVertical direction (Z), SAND BLASTED
 8-11µmVertical direction (Z), AS BUILT

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAPPR3132 / 239100

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.