MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Tetrashield™ AC1001 Polyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Product Description: Eastman Tetrashield™ AC1001 is a durable polyester resin system that improves the performance of both clearcoats and pigmented topcoats. Tetrashield™ protective resin systems are designed to enhance coating performance, reduce environmental impact, and optimize the coating process for automotive OEMs and suppliers.

Application/Uses:

  • Coatings – Automotive OEM clearcoats
  • Coatings – Automotive OEM topcoats
Key Attributes:
  • Enhanced long term weathering performance
  • Extended durability due to increased hydrolytic stability
  • Improved chemical & stain resistance
  • Improved mar/scratch resistance and toughness due to higher Tg
  • Reduced VOC and enhanced productivity due to higher solids at low viscosity

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 24 - 26 %
Viscosity 120 - 320 cP
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 8.0[mg KOH/g]
 
Descriptive Properties
ColorAPHA
Hydroxyl Number120-150[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5179 / 222373

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.