MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Rovene® 6107 Styrene Acrylic Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Rovene 6107 is a very hard, resin supported emulsion but has a minimum film forming temperature below 20°C that is designed to be used as a letdown vehicle in inks and overprint varnishes for paper and paperboard substrates. Inks formulated with this emulsion exhibit excellent ink transfer as well as excellent printability. Rovene 6107 exhibits outstanding gloss and non-blocking properties. It has good hold-out and excellent flow and leveling on paper and paperboard.

Markets: Printing and Packaging

Applications: Printing Inks, Overprint Varnishes, Digital Inks and Coatings

Related Products: Rovene 4111, Rovene 6101, Rovene 6103, Rovene 6112, Rovene 6115

Information provided by Mallard Creek Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 43 - 46 %
pH 8.1 - 9.0
Viscosity 500 - 2000 cP
 
Chemical PropertiesOriginal ValueComments
Acid Value 105Acid Number
 
Descriptive Properties
Minimum Film Formation Temperature (°C)20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMCP9937 / 250440

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.