MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro DESMODUR® MTQ25130 + BAYTEC® T20 + BAYTEC® XL B (Catalyst CATD0812-3), 90 A Polyurethane, MDI- PTMEG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccBAYTEC® T20
 1.01 g/cc1.01 g/ccBAYTEC® XL B
 1.10 g/cc1.10 g/ccDESMODUR® MTQ25130
 1.11 g/cc1.11 g/cc
Viscosity 30 cP30 cPBAYTEC® XL B
 800 cP800 cPDESMODUR® MTQ25130
 1200 cP1200 cPBAYTEC® T20
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090DIN 53505
 88
@Temperature 80.0 °C
88
@Temperature 176 °F
DIN 53505
 93
@Temperature -5.00 °C
93
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 46.0 MPa6670 psiDIN 53504
Tensile Stress at Strain 3.30 MPa
@Strain 10 %
479 psi
@Strain 10 %
DIN 53504
Elongation at Break 490 %490 %DIN 53504
100% Modulus 9.00 MPa
@Strain 100 %
1310 psi
@Strain 100 %
DIN 53504
200% Modulus 12.5 MPa
@Strain 200 %
1810 psi
@Strain 200 %
DIN 53504
300% Modulus 17.0 MPa
@Strain 300 %
2470 psi
@Strain 300 %
DIN 53504
Resilience 5757[%]; DIN 53512
Tear Strength 49.0 kN/m280 pliwith nick; ISO 34-1
 115 kN/m656 pliwithout nick; ISO 34-1
Abrasion 4545[mm3]; ISO 4649
Compression Set 27 %
@Temperature 70.0 °C,
Time 79200 sec
27 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 45.0 °C113 °FDESMODUR® MTQ25130
 45.0 °C113 °FBAYTEC® T20
 45.0 °C113 °FBAYTEC® XL B
Mold Temperature 100 °C212 °F
Pot Life 3.50 min3.50 min
 
Descriptive Properties
AppearanceliquidDESMODUR® MTQ25130
 solidBAYTEC® T20
 solidBAYTEC® XL B
Content0.05CATD0812-3 - % / total (by weight), (catalyst at the head)
 100Parts by weight of prepolymer
 12Parts by weight of BAYTEC® XL B
 12.9-13.3%NCO
 40Parts by weight of BAYTEC® T20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0530 / 202313

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.