MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polynt ArmorFlex® 953 Series HIGH GLOSS BUFFBACK® High Performance Flexible Gel Coat
Categories: Polymer; Thermoset

Material Notes: Polynt Composites’ ArmorFlex® 953 Series gel coats are high performance products formulated for the fiberglass industry. They are primarily formulated for marine and sanitary applications, but should be used in any application where water and chemical resistance are needed. ArmorFlex® 953 Series also have exceptional gloss and buffing characteristics. While offering these benefits, the ArmorFlex® 953 Series gel coats have retained the important construction application qualities expected from Polynt Composites gel coats, such as resistance to porosity, tearing, and color separation; sag resistance; consistent liquid properties; excellent patchability; and more. These all add up to higher quality appeal in FRP parts made from Polynt’s ArmorFlex® HIGH GLOSS BUFFBACK® gel coats. ArmorFlex® 953 Series gel coats have enabled customers to meet and surpass all requirements of the American National Standard for plastic bathtubs, shower receptors and shower stalls, ANSI Z124.1, .2 and .3 –1995, Sec. 6.1.1. Gel coats in the 953 Series require only the addition of the proper amount of the appropriate methyl ethyl ketone peroxide to cure. ArmorFlex® HIGH GLOSS BUFFBACK® gel coats are available in the same wide range of colors as other POLYCOR® gel coats. Standard base white ArmorFlex® is 953WJ340.

Features and Benefits:

  • Excellent water resistance for reduced osmotic blistering
  • Good chemical resistance for long, lasting durable finishes
  • Easier, quicker gloss recovery (less buffing time to achieve gloss)
  • Higher gloss recovery when polishing back aged or exposed gel coat surfaces
  • Higher gloss in patches and surrounding refinished area
  • Higher gloss recoverability from lower gloss molds

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content 33 - 37 g/lWhites
 36 - 40 g/lColors
Brookfield Viscosity 12000 - 18000 cPColors RVF #4 Spindle @ 4 rpm
 13000 - 19000 cPWhites RVF #4 Spindle @ 4 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 79.0 - 82.0 °FColors
 79.0 - 82.0 °FWhites
 
Processing PropertiesOriginal ValueComments
Cure Time 45.0 - 80.0 minColor, Lay-up Time
 45.0 - 80.0 minWhite, Lay-up Time
Gel Time 13.0 - 17.0 minColors, 100 g mass, 1.8% Arkema Luperox® DDM-9
 13.0 - 17.0 minWhites, 100 g mass, 1.8% Arkema Luperox® DDM-9
 
Descriptive Properties
Sag ResistanceGood at 20 milsColor
 Good at 20 milsWhites
Thixotropic Index5.5-7Colors
 5-7Whites

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9185 / 231780

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.