MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
High Silicon Ductile Iron at RT 4Si-0.5Mo nominal alloy content
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Subcritically annealed for 4 hours at 790°C, air cooled.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.10 - 7.20 g/ccTypical value of ductile iron
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 595 MPa
 75.0 MPa
@Temperature 700 °C
 130 MPa
@Temperature 650 °C
 275 MPa
@Temperature 540 °C
Tensile Strength, Yield 470 MPa
@Strain 0.2 %
 65.0 MPa
@Strain 0.2 %,
Temperature 700 °C
 110 MPa
@Strain 0.2 %,
Temperature 650 °C
 250 MPa
@Strain 0.2 %,
Temperature 540 °C
Elongation at Break 17 %
 35.5 %
@Temperature 540 °C
 71.5 %
@Temperature 650 °C
 75.5 %
@Temperature 700 °C
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 95.5 %
Molybdenum, Mo 0.50 %
Silicon, Si 4.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Medium-Silicon Ductile Iron, heat-resistant ductile iron
High Silicon Ductile Iron at RT 4Si nominal alloy content
High Silicon Ductile Iron at RT 4Si-2.5Mo nominal alloy content
High Silicon Ductile Iron at RT 4Si-0.9V nominal alloy content
High Silicon Ductile Iron at RT 4Si-1.0Mo nominal alloy content

MDFE28 / 12025

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.