MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SMAC SMACDISK® 1114S Damping Material
Categories: Other Engineering Material

Material Notes: Specifications - Shock & vibration insulation for:
  • Hard disk
  • Low frequency damping
  • Vehicular electronics
  • Requiring vibration isolation

Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °FSMACTANE®
 150 °C302 °FSMACSIL®
Minimum Service Temperature, Air -55.0 °C-67.0 °FSMACSIL®
 -30.0 °C-22.0 °FSMACTANE®
 
Descriptive Properties
MaterialsSMACTANE®
Max load per damper250g
Metal partsAluminum base
Weight5.3 g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SMAC SMACSONIC® Classic ST Noise and Vibration Damping
SMAC SMACTANE® SP Damping Material
SMAC SMACWRAP® ST Damping Material, 1 mm
SMAC SMACMOUNT® 2528S Damping Material
SMAC SMACMOUNT® 2112S Damping Material

PZSMAC012 / 146128

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.