MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SouthWest Nano Technologies SWeNT™ VC100 CNT Conductive Inks
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Printable conductive carbon nanotube ink

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc0.0314 lb/in³
Solids Content 0.050 - 0.10 %0.050 - 0.10 %
Filler Content 0.050 - 0.10 %0.050 - 0.10 %Carbon Nanotube (CNT)
Particle Size 0.0010 µm0.0010 µm
Viscosity 50 - 5000 cP50 - 5000 cP
Thickness 0.100 microns0.00394 mil
Surface Tension 30 dynes/cm30 dynes/cm
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 200 - 10000 ohm200 - 10000 ohm
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 95 %95 %
 
Descriptive Properties
Binder Systemnone
Conductive Filler TypeCarbon Nanotube (CNT)
Material TypeReady-To-Use Formulation
Solvent Systemamine/alcohols

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFLEXCM44 / 179446

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.