Sequel E3400 SP RXF BLACK fractional melt flow, high flexural modulus, improved scratch resistance thermoplastic polyolefin (TPO) is typically used for thermoformed exterior or interior applications that require low-temperature toughness and dimensional stability. This extrusion-grade material exhibits enhanced melt strength for a wide thermoforming processing window. Applications: Industrial, Panels & ProfilesInformation provided by LyondellBasell. |