MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Toray PMC CFRT® XTX-Orthotics XTX-UR, Ultra Rigid, Continuous Fiber Reinforced Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Toray PMC CFRT® XTX-Orthotics are lightweight, high strength laminates that are available in several rigidity types ranging from Ease Flex to Ultra Rigid.

Features:

  • Thin durable material for custom orthotics for use in a broad range of applications from dress shoes to athletics.
  • Four XTX grades are available: Ease Flex, Semi Rigid, Rigid, and Ultra Rigid.
  • Easy to mold and finish, requires no special handling.
  • Value and performance leader
  • Composite structure for thinness and high strength
  • Superior recoil and spring characteristics
  • Can be reheated and remolded
  • Unique resin designed for high resistance to cracking, impact and fatigue
  • Deep heel cups and directional rigidity for greater foot support and control
Product Type And Composition: Toray PMC CFRT® Fiber Reinforced Polypropylene Thermoplastic Biaxial Laminate (Continuous Fiber Reinforced Thermoplastic)

Information provided by Toray Performance Materials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 3000 microns
 
Descriptive Properties
Heating Time5 min400°-420°F(204-216°C)Oven
Rigidity10Factor

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTORAY8097 / 265495

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.