MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical LUPOY SC3154 PC+GF15%  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical Resistance

Application: Mobile Phone Housing and Components

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0050 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 11 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 123ASTM D785
Tensile Strength, Yield 480 kg(f)/cm²
@Thickness 3.20 mm
5mm/min; ASTM D638
Elongation at Break 25 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 900 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Flexural Modulus 31000 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Izod Impact, Notched >= 22.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 137 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 80.0 °C
@Thickness >=1.70 mm
 80.0 °C
@Thickness >=3.10 mm
UL RTI, Mechanical with Impact 80.0 °C
@Thickness >=1.70 mm
 80.0 °C
@Thickness >=3.10 mm
UL RTI, Mechanical without Impact 80.0 °C
@Thickness >=1.70 mm
 80.0 °C
@Thickness >=3.10 mm
Flammability, UL94 HB
@Thickness >=1.70 mm
 HB
@Thickness >=3.10 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 295 °CInjection Molding
Middle Barrel Temperature 285 - 300 °CInjection Molding
Front Barrel Temperature 290 - 305 °CInjection Molding
Nozzle Temperature 290 - 305 °CInjection Molding
Melt Temperature 295 - 310 °CInjection Molding
Mold Temperature 90.0 - 110 °CInjection Molding
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 3.00 - 5.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPaInjection Molding
Screw Speed 40 - 70 rpmInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Impact Grade
Entec Hypro™ F PPC-GF25 Natural Impact Polypropylene, 25% Glass Reinforced
LG Chemical Lupox® LW5102F PBT+PC+GF10%
Techmer ES HiFill® PC GF20 X 20% Glass Filled
Techmer ES HiFill® ABS GF15 BK 15% Glass Filled

PLAY537 / 148547

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.