MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Thermal Ceramics Superwool 607 Blanket AC2
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Superwool 607 Blanket AC2 is made specifically for sound absorption applications. It has excellent sound absorption characteristics, thermal stability, superior mechanical strength and vibration resistance. This product combines excellent uniformity with enhanced thermal and acoustical performance. It is flexible, easy to cut, shape and install.

Superwool 607 Blanket AC2 is made of long fibers, needled from both sides, and possesses high strength before and after heating.

Features:

  • Low biopersistence
  • Excellent sound absorption
  • Thermal stability
  • Low heat storage
  • Good resistance to tearing
  • Flexible and resilient
  • Immune to thermal shock
  • Excellent thermal insulating performance
  • Exonerated under Nota Q of Directive 97/69/EC
  • Not subject to any use restrictions under German hazardous substance regulation
  • Based on patented technology
  • Applications:

  • HRSG silencers
  • Mufflers
  • Sound Walls
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.0500 g/cc0.00181 lb/in³
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0893 W/m-K
    @Temperature 200 °C
    0.620 BTU-in/hr-ft²-°F
    @Temperature 392 °F
    ASTM C201
     0.140 W/m-K
    @Temperature 300 °C
    0.970 BTU-in/hr-ft²-°F
    @Temperature 572 °F
    ASTM C201
     0.220 W/m-K
    @Temperature 400 °C
    1.53 BTU-in/hr-ft²-°F
    @Temperature 752 °F
    ASTM C201
     0.320 W/m-K
    @Temperature 500 °C
    2.22 BTU-in/hr-ft²-°F
    @Temperature 932 °F
    ASTM C201
     0.440 W/m-K
    @Temperature 600.0 °C
    3.05 BTU-in/hr-ft²-°F
    @Temperature 1112 °F
    Shrinkage <= 1.5 %
    @Temperature 1000 °C,
    Time 86400 sec
    <= 1.5 %
    @Temperature 1832 °F,
    Time 24.0 hour
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 <= 0.30 %<= 0.30 %
    CaO+MgO 25 - 40 %25 - 40 %
    SiO2 60 - 70 %60 - 70 %
     
    Descriptive Properties
    Airflow Resistance, Rayls/m10000-15000 , ASTM C522
    Leachable chlorides, ppm<10

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM298 / 2618

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.